What defines 302HQ's chemical composition?
It contains 17-19% chromium, 9-11% nickel, low carbon (<=0.06%), and added copper (1.5-3.5%). The low carbon and copper additions improve cold formability, making it ideal for cold heading operations.
How does 302HQ perform in cold heading processes?
302HQ is highly ductile, resisting cracking during cold heading, threading, and forming. It maintains strength after forming, making it a top choice for high-quality fasteners like bolts and screws.
It offers excellent corrosion resistance, similar to 304, with the low carbon content reducing carbide precipitation. It resists rust in atmospheric conditions and fresh water, suitable for outdoor fasteners.
How does 302HQ compare to 304 in mechanical properties?
302HQ has slightly lower tensile strength than 304 but higher ductility, with elongation up to 45%. This balance makes it better for cold forming while retaining enough strength for structural fasteners.
What are 302HQ's typical applications?
Commonly used in high-quality fasteners, including bolts, nuts, and screws, especially in automotive and construction. It's also found in precision parts requiring cold forming, where ductility and corrosion resistance are key.